MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AGC Lumiflon LF-600X Solvent Soluble Fluoropolymer
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. LF-600X has a high OH functionality and can be crosslinked with polyisocyanate and provides coating with a high gloss and durability. It can be used to make a flexible film.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Solids Content 50 %50 %
Viscosity Measure 1300 - 3700 cSt1300 - 3700 cSt
Molecular Weight 20000 g/mol20000 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.000.00
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 20.0 °C68.0 °F
 
Descriptive Properties
AppearanceTransparent
OH Value mg KOH/g57
SolventXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC LUMIFLON® LF-600X Fluoropolymer Resin
A. Schulman BMC 1412 Flame and Track Resistant
Schott CONTURAX® Pro Borosilicate Glass
Schott CONTURAX® Borosilicate Glass
Röchling Glastic BMC 1412 GTP Glass-Reinforced Polyester

PAGC08 / 22967

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.