MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Mersolat® H95 Plastic Additive, Emulsifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Secondary Alkane Sulfonates (SAS) which are used as raw materials for textile processing chemicals, leather auxiliaries, detergents and cleaning products, as anionic emulsifier for emulsions polymerizations and as antistatic agent for plastic materials.

Chemical composition: Mixture of primarily secondary sodium alkyl sulfonates with an average chain length of C15.

CAS Reg. No. 68188-18-1

Applications:
Raw material for detergents, wetting agents textile processing chemicals and leather auxiliaries-Mersolat® H can be used as an anionic surfactant for the production of particularly liquid and highly-concentrated paste-like detergents and wetting agents for the textile and leather industry as well as of alkaline and acid industrial cleansers, disinfectant cleansers, and house hold detergents and cleaning agents. Mersolat® H is comparatively stable against acids, alkali, and electrolytes.

Stabilizing dispersions-Because of its excellent emulsifying properties, Mersolat® H is suitable for use in the processing of synthetic lattices, natural latex, and acrylate dispersions. Even small addition rates (0.2 – 3.0%) allow the production of high-percentage plastic dispersions (45 – 50%) with a high stability.
High grade anionic emulsifier for emulsion polymerization-Mersolat® H is an auxiliary for the manufacture and stabilization of emulsions. It is used as an anionic emulsifier in the emulsion polymerization of vinyl chloride, acrylonitrile, butadiene, styrene, acrylates, other monomers and their mixtures, especially for the manufacture of ABS. Dispersions with a high stability which form little scale in the reactors can be obtained with only low additions (0.2 – 3.0%). Mersolat® H has proven itself effective in both continuous (addition approx. 2%) and discontinuous (addition approx. 1%) polymerization of E-PVC. The absence of double bonds means that the emulsifier does not act as a radical interceptor which ensures an easily reproducible reaction process

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 8.0 - 10.58.0 - 10.5
Iodine Absorption Number <= 0.10<= 0.10<0.1g l/100g
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.2 %<= 1.2 %Karl Fischer
Shelf Life 24.0 Month
@Temperature >=20.0 °C
24.0 Month
@Temperature >=68.0 °F
 
Descriptive Properties
AppearanceWhite to pale yellow flakes
Content<1%Neutral oil
 <3.5%Sodium chloride
 >95%Active substance
 0.1 percentSodium sulfate
 12 percentDi- and poly-sulfonates
 83 percentMonosulfonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Mersolat® H68 Plastic Additive, Emulsifier
Lanxess Mersolat® H40 Plastic Additive, Emulsifier
Lanxess Mersolat® H30 Plastic Additive, Emulsifier

PLANY8898 / 209290

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.