System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Techmer ES HiFill® HDPE GF15 15% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Glass fiber Filled
Material Notes:
Availability: North America
Forms: Pellets
Filler/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight
Information provided by TP Composites, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.05
g/cc
0.0379
lb/in³
ASTM D792
Water Absorption
0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow
0.0070
cm/cm
@Thickness 3.17 mm
0.0070
in/in
@Thickness 0.125 in
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
80
80
ASTM D785
Tensile Strength, Yield
34.5
MPa
5000
psi
ASTM D638
Elongation at Break
3.0 %
3.0 %
ASTM D638
Flexural Strength
55.2
MPa
8000
psi
ASTM D790
Flexural Modulus
4.07
GPa
590
ksi
ASTM D790
Izod Impact, Notched
0.801
J/cm
@Thickness 3.17 mm
1.50
ft-lb/in
@Thickness 0.125 in
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+15
ohm-cm
1.00e+15
ohm-cm
ASTM D257
Dielectric Strength
11.8
kV/mm
300
kV/in
Method A (Short-Time); ASTM D149
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
54.0
µm/m-°C
30.0
µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
129
°C
265
°F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
121
°C
250
°F
Unannealed; ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Avient Edgetek® PE-10GF/000 High Density Polyethylene (HDPE), Glass Filled
Techmer ES HiFill® HDPE GF10 CC 10% Glass Filled
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
Techmer ES HiFill® HDPE GF15 50100 15% Glass Filled
Techmer ES HiFill® HDPE E GF40 40% Glass Filled
PTPC0050 / 135988
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.