MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rogers Arlon 48B12R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave: Polyethylene
Side 1: Cured Silicone Rubber
Substrate: Style 1080 Fiberglass

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns2.00 milSide 1; Arlon SQA-TMS-003
 63.5 microns2.50 milInterleave
 76.2 microns3.00 milSubstrate; Arlon SQA-TMS-003
 127 microns5.00 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555Silicone Property; ASTM D2240
Tensile Strength 6.72 MPa975 psiSilicone Property; ASTM D412
Elongation at Break 275 %275 %Silicone Property; ASTM D412
Tear Strength 9.64 kN/m55.0 pliDie B, Silicone Property; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.4 kV/mm900 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
Flammability Test >= 0.50>= 0.50[sec], Flame and Glow; FAR 25.853 App.F, P.1,.Aii
 >= 0.50>= 0.50[in], Char Length; FAR 25.853 App.F, P.1,.Aii
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 60.0 Month
@Temperature 21.1 °C
60.0 Month
@Temperature 70.0 °F
From date of manufacture
 
Descriptive Properties
ColorRed
 RedSubstrate
Total Product Weight (oz/yd2)4.3Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Trelleborg S765 Silicone Rubber
Rogers Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon R34572R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 51426R015 0.015" Cured/Uncured Silicone Rubber with Fiberglass Substrate

PARL230 / 125416

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.