MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a good balance of transparency, strength and fluidity (methyl methacrylate butadiene styrene), "TE Series/CL Series," transparent ABS resins with excellent color attributes and tensile strength are available (among others).

Applications

TX is used for:

  • flat display substrates
  • optical components
  • miscellaneous goods.
TP/TH are used for:
  • food package sheeting as well as in manufacturing
  • electronic equipment and components
  • miscellaneous goods
TE/CL are for:
  • electronic equipment and components
  • information equipment components
  • AV equipment, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Density 1.086 g/cc0.03923 lb/in³ISO 1183
Melt Flow  3.1 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.1 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 76 g/10 min
@Load 10.0 kg,
Temperature 220 °C
76 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 3434ISO 2039-2
Tensile Strength at Break 36.0 MPa5220 psi50mm/min; ISO 527-2
 42.0 MPa6090 psi50mm/min; ASTM D638
Elongation at Break 30 %30 %50mm/min; ISO 527-2
Tensile Modulus 4.70 GPa682 ksi50mm/min; ISO 527-1
Flexural Strength 68.0 MPa9860 psiISO 178
 69.0 MPa10000 psi2mm/min; ASTM D790
Flexural Modulus 2.22 GPa322 ksi2mm/min; ASTM D790
 2.25 GPa326 ksi2mm/min; ISO 178
Izod Impact Resistance 9.50 J/cm²45.2 ft-lb/in²
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FISO 75-2
 72.0 °C162 °FASTM D648
Vicat Softening Point 84.0 °C183 °F50N; ISO 306
Flammability, UL94 HBHB
 
Optical PropertiesMetricEnglishComments
Haze 2.6 %
@Thickness 2.00 mm
2.6 %
@Thickness 0.0787 in
ISO 14782
Transmission, Visible 91 %
@Thickness 2.00 mm
91 %
@Thickness 0.0787 in
ISO 13468-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
Nitriflex Nitrimpact 1300 MBS Modifier
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
INEOS Styrolution Zylar® 650 MBS

PDENK013 / 29677

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.