MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omni Plastics OmniPro™ HPP CCF40 Homopolymer Polypropylene, 40% Calcium carbonate filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Calcium Carbonate (CaCO3) Filler

Material Notes: 40% CaCO3 reinforced; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Filler Content 40 %40 %ASTM D2584
Melt Flow 10 g/10 min10 g/10 minASTM D1248
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Flexural Strength 41.0 MPa5950 psiASTM D790
Flexural Modulus 2.275 GPa330.0 ksiASTM D790
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
0.993 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
@Thickness 3.17 mm
235 °F
@Thickness 0.125 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
@Thickness 3.17 mm
160 °F
@Thickness 0.125 in
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Omni Internal Testing
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 249 °C400 - 480 °F
Middle Barrel Temperature 216 - 260 °C420 - 500 °F
Front Barrel Temperature 216 - 260 °C420 - 500 °F
Nozzle Temperature 216 - 260 °C420 - 500 °F
Melt Temperature 216 - 260 °C420 - 500 °F
Mold Temperature 26.7 - 60.0 °C80.0 - 140 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omni Plastics OmniTuff™ HPP CCF40 Homopolymer Polypropylene Calcium Carbonate Filled
Omni Plastics OmniPro™ HPP CCF30 Homopolymer Polypropylene, 30% Calcium carbonate filled
Omni Plastics OmniPro™ HPP CCF20 Homopolymer Polypropylene, 20% Calcium carbonate filled
Omni Plastics OmniPro™ HPP CCF10 Homopolymer Polypropylene, 10% Calcium carbonate filled
A. Schulman Matrixx CPP2B40 Polypropylene Copolymer, 40% Calcium Carbonate Filled

POMNI5071 / 185217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.