MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Monmouth Rubber & Plastics Superbounce 90 NEO/SBR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Monmouth Rubber & Plastics Corp.

Key Words: Polychloroprene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density >= 0.721 g/cc>= 0.0260 lb/in³
Water Absorption <= 1.0 %<= 1.0 %ASTM D1056
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 80 - 9080 - 90ASTM D2240
Tensile Strength 8.791 MPa1275 psiASTM D2000
Elongation at Break 862 %862 %ASTM D2000
Compressive Strength 0.517 - 0.586 MPa75.0 - 85.0 psi25%; ASTM D1056
Tear Strength 42.1 kN/m240 pliDie C; ASTM D3575 Suf. G
Compression Set  8.0 %
@Time 86400 sec
8.0 %
@Time 24.0 hour
 10 %
@Time 3600 sec
10 %
@Time 1.00 hour
 14 %
@Time 60.0 sec
14 %
@Time 0.0167 hour
 14 %
@Time 299 sec
14 %
@Time 0.0830 hour
 20 %
@Time 5.00 sec
20 %
@Time 0.00139 hour
 
Descriptive Properties
C/D Heat Aging0.37 days @158°F, Change; ASTM D1056
ColorBlack
Compression Recovery90%5 sec; ASTM D1056
 93%60 sec; ASTM D1056
 95%5 mins; ASTM D1056
 95%60 mins; ASTM D1056
 96%24 hrs; ASTM D1056
Fluid Immersion0.2Oil, Ref Fuel B, ASTM D1056
G Max Rating Vertical energy input163 G's8.8/FT Second; ASMT F1292-99
 235 G's10.5/FT Second; ASMT F1292-99
 86 G's6.6/FT Second; ASMT F1292-99

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Poly-L-lactide (PLLA)
Denka Neoprene W Polychloroprene Rubber
Denka Neoprene GNA Polychloroprene
Denka Neoprene 671A Polychloroprene

PMONM036 / 160838

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.