MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mitsubishi Chemical Advanced Materials Proteus® PP, ProKnob Finish Natural Homopolymer Polypropylene (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes:

  • High impact resistance strength
  • Better resistance to cracking at low temperatures than Homopolymer Polypropylene
  • More pliable than homopolymer
  • Meets food handling guidelines
  • Chemical- and corrosion-resistant
  • No moisture absorption
  • FDA and 3-A Dairy CompliantAppropriate for applications to 180°F (82°C)
  • Resists most acids, alkalis and solvents
  • Meets FDA 21CFR 177.1520
  • Thermoforming performance
  • USDA, NSF and 3-A Dairy Complaint (natural color only)

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7878ASTM D2240
Tensile Strength 33.1 MPa4800 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 11 %11 %ASTM D638
Tensile Modulus 1.31 GPa190 ksiASTM D638
Flexural Strength 33.1 MPa4800 psiASTM D790
Flexural Modulus 1.34 GPa195 ksiASTM D790
Compressive Strength 34.5 MPa5000 psi10% Def.; ASTM D695
Compressive Modulus 1.38 GPa200 ksiASTM D695
Izod Impact, Notched 0.641 J/cm1.20 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.250.25Dry vs. Steel; QTM55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 °C327 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYes
Canada AG NoNo
FDA YesYes
NSF YesYes
USDA YesYes
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic UnacceptableUnacceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Proteus™ Homopolymer PP White Polypropylene
Mitsubishi Chemical Advanced Materials Proteus™ Copolymer PP Natural Polypropylene
Overview of materials for Polypropylene, Molded
Mitsubishi Chemical Advanced Materials Proteus™ HDPE High Density Polyethylene
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene

P1SMP54 / 20179

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.