MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DAK Americas Laser+® C K62A PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Laser+® C (K62A) is a unique copolymer particularly suited for use in both the BCF (bulk continuous filament) production of fibers and custom PET container application where clarity and neutral color are desired. It is a low intrinsic viscosity (IV) product that gives the end user clarity and offers excellent processing and consistency.

Typical Properties: The polymer properties are designed for optimized filament extrusion, fiber spinning and performance. BI-orientation of Laser+® C (K62A) by injection/stretch blow molding provides optimal barrier and mechanical properties, including good vacuum performance. It performs well in BCF and single- and two-stage processes used in the manufacturing of PET containers.

Certification: Laser+® C (K62A) is ideally suited for food packaging applications and is considered in compliance with the Food and Drug Administration (FDA) Food Contact Notification (FCN) 000635, and Health Canada Health Products and Food Branch (HPFB) file KS 05103105 for PET polymers.

Information provided by DAK Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.870 g/cc0.0314 lb/in³DAK-QAR-SOP-0018
Particle Size 3000 µm3000 µmFlat Cylinder Shape; DAK-QAR-SOP-0017
Particle Mesh Size 24 Mesh24 MeshFines: <0.1%, as packaged; DAK-QAR-SOP-0014
Viscosity Test 74 - 78 cm³/g0.74 - 0.78 dl/gIntrinsic; DAK-QAR-SOP-0012
Crystallinity >= 50 %>= 50 %DAK-QAR-SOP-0016
 
Thermal PropertiesMetricEnglishComments
Melting Point 246 °C475 °Fnominal; DAK-QAR-SOP-0016
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %DAK-QAR-SOP-0013; as packaged
 
Descriptive Properties
Chip Size48-58 chips/gnominal, DAK-QAR-SOP-0015
Color-5- -1 CIEb*, DAK-QAR-SOP-0011
 85-89 CIEL*, DAK-QAR-SOP-0011

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DAK Americas Laser+® C 4800 B66A PET
DAK Americas Laser+® C E61A PET
DAK Americas Laser+® B90B PET
DAK Americas Laser+® C C61A PET
DAK Americas Laser+® B90A PET

PDAKA010 / 147985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.