MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Cerablok 800 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Cerablok slabs are made from refractory and mineral fibres, natural refractory components and a small amount of organic binder. Thanks to the high fibre content, Cerablok are strong, lightweight and thermal shock resistant. All grades of Cerablok are water repellent throughout to prevent absorption of water or concrete binders. Thicknesses over 50mm are obtained by gluing two standard slabs together.

Applications:

  • Back up for dense or insulating refractory products, in the following industries (among others).
  • Galvanisation
  • Cement works
  • Furnaces
  • Stoves and driers
  • Glass works (lehrs, feeders, regenerators)
  • Aluminium: electrolytic reduction cells (Cerablok 800 and 1000)
  • Petrochemical industry (Cerablok 800 and 1000)

    Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.320 g/cc0.0116 lb/in³50% RH
Loss On Ignition 5.5 %5.5 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.000700 GPa0.102 ksi23°C, 50% RH
Compressive Strength 0.350 MPa50.8 psiat 10% reduction in thickness, 23°C, 50%RH
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0750 W/m-K
@Temperature 300 °C
0.521 BTU-in/hr-ft²-°F
@Temperature 572 °F
 0.0800 W/m-K
@Temperature 400 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.0930 W/m-K
@Temperature 500 °C
0.645 BTU-in/hr-ft²-°F
@Temperature 932 °F
 0.112 W/m-K
@Temperature 600 °C
0.777 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.700 W/m-K
@Temperature 200 °C
4.86 BTU-in/hr-ft²-°F
@Temperature 392 °F
Maximum Service Temperature, Air <= 800 °C<= 1470 °F
Shrinkage <= 0.80 %
@Time 86400 sec
<= 0.80 %
@Time 24.0 hour
isothermal heating at classification temp
 
Descriptive Properties
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Z-Blok 1 Modules Kaowool S/Cerablanket
Morgan Advanced Ceramics Kaowool Millboard 830 Thermal Ceramic
Morgan Advanced Ceramics JM 2600 Thermal Ceramic
Morgan Advanced Ceramics Cerasil ™ Alumino Silicate 223U Alumino Silicate Ceramic
Morgan Advanced Ceramics Ceraboard 115 Fiber

CMORF6507 / 203291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.