MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Shinil Chemical SHINCON MPPO Electro Conductive Polymer
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's patented conductive filler dispersion technology with variety of engineering polymers and their alloys to impart permanent static dissipative to electrically conductive property to thermoplastics. SHINCON contains multiwall carbon nanotube (MWCNT), carbon black (CB), and carbon fiber (CF) as a conductive filler. SHINCON are used in injection molding, film or sheet extrusion for the applications where the desired level of conductivity and unique mechanical property are important. A wide range of the surface resistaivity is obtained by SHINCON formulations for the parts and devices depending upon customer needs and applications.

    Feature and Benefits
  • Permanent electro conductivity
  • Maintain the physical properties of base resin
  • No particulates (CNT product)
  • Lighter weight
  • Recyclability
  • Easy processing
  • Improved surface
  • Cost effective

Grade/Application: IC Tray

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 108 MPa15600 psi
Flexural Strength 186.39 MPa27034 psi
Flexural Modulus 8.63 GPa1250 ksi
Izod Impact, Notched 0.686 J/cm1.29 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 200000 ohm-cm200000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Beijing Chemical Industry KAIFA® M104 MPPO Resin
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO
Beijing Chemical Industry KAIFA® M106N MPPO Resin
Beijing Chemical Industry KAIFA® M106 MPPO Resin

PSHINL13 / 104015

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.