KEP Kepital® TX-11H Acetal Copolymer, Special lubricant package
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, Unreinforced
Material Notes:
High viscosity, lubricant package grade. TX-11H is suitable for use requiring reduced wear noise, and a good friction & wear resistance without sacrificing mechanical properties.
Information provided by KEP Americas.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.40
g/cc
0.0506
lb/in³
ISO 1183
Water Absorption
0.20 %
0.20 %
ISO 62
Linear Mold Shrinkage, Flow
0.020
cm/cm
0.020
in/in
t = 3 mm
Melt Flow
5.0
g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength
64.0
MPa
9280
psi
50 mm/min; ISO 527
Elongation at Break
40 %
40 %
50 mm/min; ISO 527
Elongation at Yield
12 %
12 %
50 mm/min; ISO 527
Flexural Strength
86.0
MPa
12500
psi
ISO 178
Flexural Modulus
2.55
GPa
370
ksi
ISO 178
Charpy Impact, Notched
0.800
J/cm²
3.81
ft-lb/in²
ISO 179
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+16
ohm-cm
1.00e+16
ohm-cm
IEC 60093
Surface Resistance
1.00e+16
ohm
1.00e+16
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
CTE, linear
130
µm/m-°C
72.2
µin/in-°F
ISO 11359
Melting Point
168
°C
334
°F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi)
97.0
°C
207
°F
ISO 75
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
KEP Kepital® TX-21 Acetal Copolymer, Special lubricant package
KEP Kepital® FM2520S Acetal Copolymer, MoS2 filled
KEP Kepital® TS-25H Acetal Copolymer, Silicone Filled
Kolon KOCETAL® SO301 Wear Modified Acetal Resin
KEP Kepital® TX-31 Acetal Copolymer, Special lubricant package
PKEP9962 / 185638
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.