System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NuSil CF3-3521 Fluorosilicone
Categories:
Polymer
;
Thermoset
;
Silicone
Material Notes:
General Purpose: Thermally Conductive
Comments: Liquid Injection Molding, Fuel Resistant
Cure System: Platinum
Information provided by NuSil
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.26
g/cc
1.26
g/cc
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
30
30
Tensile Strength at Break
4.80
MPa
696
psi
Elongation at Break
360 %
360 %
Processing Properties
Metric
English
Comments
Extrusion Rate
90.0
g/min
90.0
g/min
A
150
g/min
150
g/min
B
Cure Time
30.0
min
@Temperature 150 °C
0.500
hour
@Temperature 302 °F
Working Life
720
min
720
min
Descriptive Properties
Color
Translucent
Mix Ratio
1:1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
NuSil GEL-3500 Fluorosilicone
NuSil CF5-3521-2 Fluorosilicone
NuSil CF2-3521-2 Fluorosilicone
NuSil CF2-3521 Fluorosilicone
NuSil CF1-3510 Fluorosilicone
PNUSIL080 / 141804
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.