C.O.I.M. PLAXTER® P 70 Polymeric Plasticizer
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
;
Polymer
;
Thermoplastic
Material Notes:
Description:
Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.
Information provided by P.A.T. Products, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
550
-
700
cP
@Temperature 35.0 °C
550
-
700
cP
@Temperature 95.0 °F
Dynamic viscosity
Chemical Properties
Metric
English
Comments
Acid Value
1.0
1.0
mgKOH/g
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
73
73
Tensile Strength, Yield
25.06
MPa
3635
psi
Elongation at Break
237 %
237 %
100% Modulus
8.81
MPa
@Strain 100 %
1280
psi
@Strain 100 %
Optical Properties
Metric
English
Comments
Gardner Color Number
3.0
3.0
Descriptive Properties
Efficiency concentration PHR
42.5
N OH value (max)
20
mg KOH/g
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
C.O.I.M. PLAXTER® P 90 Polymeric Plasticizer
C.O.I.M. PLAXTER® P 80 Low Viscosity Polymeric Plasticizer
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer
C.O.I.M. PLAXTER® P 64 Polymeric Plasticizer
C.O.I.M. PLAXTER® P 42 Polymeric Plasticizer
PCOIM092 / 28695
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.