Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance. Applications: Blow molded containers with capacities ranging a few milliliters up to 20 liters, Sheet CAS No. 9002-88-4 Information provided by LG Chemical |