MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Circalok™ EP-937 Epoxy Board Level Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: LORD Thermoset™ EP-937 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/cc
Brookfield Viscosity 39000 - 56800 cP
@Temperature 25.0 °C
39000 - 56800 cP
@Temperature 77.0 °F
Spindle 6 @ 10rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 88 - 9488 - 94
Modulus of Elasticity 1.00 GPa145 ksiDMA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm
@Temperature 25.0 °C
1.00e+15 ohm-cm
@Temperature 77.0 °F
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 45.0 µm/m-°C25.0 µin/in-°FBelow Tg; TMA
Glass Transition Temp, Tg 125 °C257 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time 20.0 min
@Temperature 150 °C
0.333 hour
@Temperature 302 °F
Pot Life 40320 min
@Temperature 25.0 °C
40320 min
@Temperature 77.0 °F
Gel Time 3.00 min
@Temperature 150 °C
3.00 min
@Temperature 302 °F
Shelf Life 6.00 Month
@Temperature 0.000 - 5.00 °C
6.00 Month
@Temperature 32.0 - 41.0 °F
 
Descriptive Properties
AppearanceBlack
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Devcon Plastic Steel® Putty (A) Epoxy
3M Scotch-Weld™ 2216 B/A Gray Two-Part Epoxy Adhesive 2216 B/A Gray

PLORD095 / 86103

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.