MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyram RamOfin PPH308G6 Polypropylene, 30% Glass Fiber, Impact Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Glass Reinforced, Impact Modified

Material Notes: 30% Glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inISO 2577
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115
Tensile Strength, Yield 95.0 MPa13800 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Tensile Modulus 6.00 GPa870 ksiISO 527
Flexural Strength 115 MPa16700 psiISO 178
Flexural Modulus 5.90 GPa856 ksiISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180
Charpy Impact Unnotched 7.50 J/cm²35.7 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FISO 11357
Maximum Service Temperature, Air 110 °C230 °FContinuous use
 140 °C284 °FShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 153 °C307 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Flame Spread 40 mm/min1.6 in/minFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Polifor® L30 GF/30 Reinforced Polypropylene
Celanese SO.F.TER Polifor® L3 GF/30 Reinforced Polypropylene
Buckeye Polymers BP RPP 3009 GK3 BLK Polypropylene, Glass Filled
Avient Maxxam™ NT-818.B001-8000 Polypropylene
Adell RR-39 Polypropylene Copolymer; 43% Glass Reinforced, High Impact

PPOLYR929 / 126726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.