MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parson Adhesives PARTITE® 9326 Acrylic Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: PARTITE 9326 a no-mixing, high viscosity combined with fast cure speed structural adhesive for wide variety of industrial assembly applications. It bonds wide range of materials with the use of Activator 1649.

FEATURE:

  • Adhesive is applied to one surface and Activator to the other; press together and fixing is achieved within few minutes.
  • Excellent resistance to gasoline, lubricants, water, solvents, etc.
APPLICATIONS:
  • Ideal for bonding Metals, Ferrite, Plated Metals, etc.
  • Widely used for electric motors, loudspeaker and Jewelry assembly.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Brookfield Viscosity 10000 - 24000 cP10000 - 24000 cPRVT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 32.8 MPa>= 4750 psiISO 37
Elongation at Break 127 %127 %ISO 37
Tensile Modulus >= 0.310 GPa>= 45.0 ksiASTM D638
Shear Strength >= 13.8 MPa>= 2000 psiSteel to Steel, grit blasted; ISO 4587
Peel Strength >= 2.10 kN/m>= 12.0 pliISO 11339
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.54.5DIN 53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
Flash Point >= 92.0 °C>= 198 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.00 - 2.00 min0.0167 - 0.0333 hourSpeed
 1440 min24.0 hourFull
 
Descriptive Properties
ColorClear Amber Liquid
CompositionUrethane Methacrylate
Gap Filling0.05-0.5 mmCured
Initial Strength Retained (%)100Motor Oil for 500 hrs at 125°C
 100Motor Oil for 1000 hrs at 125°C
 40Water/Glycol for 500 hrs at 87°C
 40Water/Glycol for 1000 hrs at 87°C
 50Acetone for 1000 hrs at 22°C
 55Acetone for 500 hrs at 22°C
 75Ethanol for 1000 hrs at 22°C
 80Ethanol for 500 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® Output™ 315 Acrylic Adhesive
ASTM A500 Steel, grade B, round structural tubing
ASTM A500 Steel, grade A, Round Structural Tubing
Henkel Loctite® Output™ 383 Acrylic Adhesive
Humiseal 1B31 Acrylic Conformal Coating

PPARSN087 / 186530

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.