MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese 1703 FDA Nylon 6/6, 25% Glass-Fiber Reinforced, Dry As Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: FDA compliance, heat stabilized

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Water Absorption 1.0 %1.0 %24 hour immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Tensile Strength, Ultimate 172 MPa24900 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 260 MPa37700 psiASTM D790
Flexural Modulus 7.60 GPa1100 ksiASTM D790
Shear Strength 84.0 MPa12200 psiASTM D732
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 28.8 µm/m-°C
@Temperature 20.0 °C
16.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 257 °C495 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 257 °C495 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese 1500 FDA Nylon 6/6, 33% Glass-Fiber Reinforced, Dry As Molded
Celanese 1700 FDA Nylon 6/6, 25% Glass-Fiber Reinforced, Dry As Molded
Celanese 1703 FDA Nylon 6/6, 25% Glass-Fiber Reinforced, at 50% RH
Celanese 1700 FDA Nylon 6/6, 25% Glass-Fiber Reinforced, at 50% RH
Celanese 1600 FDA Nylon 6/6, 40% Glass-Fiber Reinforced, at 50% RH

PHCT77 / 45717

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.