MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Leaded High-Strength Yellow Brass, UNS C86700, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal and Sand.

Applications: High strength free-machining manganese bronze. Valve stems.

Classified under: Manganese and leaded manganese bronze alloys. ASTM B584; formerly ASTM B132-B

Data typical for as-sand-cast separately cast test bar (M01 temper). Alloy does not respond to heat treating

Key Words: Leaded Manganese Bronze, ASTM B584; ASTM B132-B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.32 g/cc0.301 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1551553000 kg
Hardness, Rockwell B 8080
Tensile Strength, Ultimate 585 MPa84800 psi
Tensile Strength, Yield 290 MPa
@Strain 0.5 %
42100 psi
@Strain 0.5 %
Elongation at Break 20 %20 %in 50 mm
Modulus of Elasticity 105 GPa15200 ksi
Machinability 55 %55 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000005387 ohm-cm
@Temperature 20.0 °C
0.000005387 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.6 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.376 J/g-°C0.0899 BTU/lb-°F
Thermal Conductivity 2.45 W/m-K17.0 BTU-in/hr-ft²-°F
Melting Point 860 - 880 °C1580 - 1620 °F
Solidus 862 °C1580 °F
Liquidus 880 °C1620 °F
Shrinkage 2.1 %2.1 %Patternmaker's Shrinkage (1/4 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 260 °C500 °FStress-Relieving Temperature
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.0 - 3.0 %1.0 - 3.0 %
Copper, Cu 55 - 60 %55 - 60 %
Iron, Fe 1.0 - 3.0 %1.0 - 3.0 %
Lead, Pb 0.50 - 1.5 %0.50 - 1.5 %
Manganese, Mn 1.0 - 3.5 %1.0 - 3.5 %
Nickel, Ni <= 1.0 %<= 1.0 %
Tin, Sn <= 1.5 %<= 1.5 %
Zinc, Zn 30 - 38 %30 - 38 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel-Manganese Bronze, UNS C86800, Copper Casting Alloy
Leaded High-Strength Yellow Brass, UNS C86400, Copper Casting Alloy
Manganese Bronze, UNS C86100, Copper Casting Alloy
High-Strength Yellow Brass, UNS C86500, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy

MC86700b1 / 11917

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.