System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Lanxess Pocan® B 3225 Z 000000 PBT, 20% Glass Fiber
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Material Notes:
PBT, 20% glass fibers, injection molding, impact modified
The Pocan® product line was transferred to Envalior, but this product was discontinued prior to that transaction.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.45
g/cc
0.0524
lb/in³
ISO 1183
Water Absorption
0.40 %
0.40 %
Test Sim. to ISO 62
Moisture Absorption at Equilibrium
0.10 %
0.10 %
23°C/50% R.H.; Test Sim. to ISO 62
Melt Flow
26
g/10 min
@Load 2.16 kg,
Temperature 260 °C
26
g/10 min
@Load 4.76 lb,
Temperature 500 °F
Estimated using room temperature density; ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
115
MPa
16700
psi
ISO 527-1/-2
Elongation at Break
3.3 %
3.3 %
ISO 527-1/-2
Tensile Modulus
6.70
GPa
972
ksi
ISO 527-1/-2
Charpy Impact Unnotched
6.00
J/cm²
@Temperature 23.0 °C
28.6
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
1.00
J/cm²
@Temperature 23.0 °C
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
30.0
µm/m-°C
16.7
µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
50.0
µin/in-°F
ISO 11359-1/-2
Melting Point
225
°C
437
°F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi)
200
°C
392
°F
ISO 75-1/-2
Flammability, UL94
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
Oxygen Index
20 %
20 %
ISO 4589-1/-2
Processing Properties
Metric
English
Comments
Melt Temperature
260
°C
500
°F
Injection Molding; ISO 294
Mold Temperature
80.0
°C
176
°F
Injection Molding; ISO 10724
Descriptive Properties
Additives
Release agent
Features
High impact or high impact modified
Form
Pellets
ISO Short Name
ISO 7792-1-PBT,GHMPR,09-070,GF20
Processing
Injection molding
Region
Asia Pacific
Europe
Near East/Africa
North America
South and Central America
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Pocan® B 3225 901510 PBT, 20% Glass Fiber
PLANX0857 / 99072
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.