MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE

Material Notes: Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydrolytic stability, oil, fuel and solvent resistance. It is supplied uncolored in pellet form.

Availability: North America

Features: Fuel Resistant, Good Toughness, Oil Resistant, Hydrolytically Stable, Solvent Resistant, Good Abrasion Resistance

Appearance: Colorless

Forms: Pellets

Processing Method: Injection Molding and Extrusion

Information provided by Alliance Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 35.0 MPa5080 psiASTM D412
Tensile Stress at Strain  4.00 MPa
@Strain 100 %
580 psi
@Strain 100 %
ASTM D412
 7.03 MPa
@Strain 300 %
1020 psi
@Strain 300 %
ASTM D412
Elongation at Break 610 %610 %ASTM D412
Tear Strength 100 kN/m571 pliDie C; ASTM D412
Taber Abrasion, mg/1000 Cycles 2323ASTM D1044
Abrasion 1515mm3; DIN 53516
Compression Set  23 %
@Temperature 22.8 °C,
Time 79200 sec
23 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D3995B
 37 %
@Temperature 70.0 °C,
Time 259000 sec
37 %
@Temperature 158 °F,
Time 72.0 hour
ASTM D3995B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FASTM D1525
Brittleness Temperature -40.0 °C-40.0 °FASTM D746
Flammability, UL94  HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 - 205 °C392 - 401 °FInjection
 205 °C401 °FGate Temperature; Extrusion
Rear Barrel Temperature 175 °C347 °FInjection
Middle Barrel Temperature 190 °C374 °FInjection
Front Barrel Temperature 205 °C401 °FInjection
Nozzle Temperature 205 - 210 °C401 - 410 °FInjection
Zone 1 175 °C347 °FExtrusion
Zone 2 190 °C374 °FExtrusion
Zone 3 205 °C401 °FExtrusion
Die Temperature 205 °C401 °FExtrusion
Mold Temperature 25.0 - 60.0 °C77.0 - 140 °FInjection
Injection Velocity >= 10.0 mm/sec>= 0.394 in/secInjection
Drying Temperature 85.0 °C185 °FInjection
 85.0 °C185 °FExtrusion
Dry Time 4.00 hour4.00 hourInjection
 4.00 hour4.00 hourExtrusion
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psiInjection
Clamp Pressure 40.0 - 70.3 MPa5800 - 10200 psiInjection
Screw Speed 60 - 200 rpm60 - 200 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 4085A Thermoplastic Polyurethane Elastomer

PAPS082 / 159455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.