MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Chemlam® RL® RL7000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sintered PTFE for low friction, flame resistance, chemical and barrier properties. Chemlam® RL® series is a high performance composite that has desirable elongation properties, and is easy to fabricate using standard techniques such as sewing for conversion to finished articles.

RL 7000
Reinforcement: Polyester/Cotton Blend. All data based on a 0.012 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.001 g/cc1.001 g/ccWoven Density
 
Mechanical PropertiesMetricEnglishComments
Tear Strength Test 1212Lbs./In. Propagation Tear Strength in fill/transverse direction
 2020Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 21.9 kN/m125 pliFill/Transverse direction
 30.7 kN/m175 pliWarp/Longitudinal direction
 
Descriptive Properties
ColorBlack/White
Weight (oz/yd^2)9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Chemlam® RL® RL6000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate
Saint-Gobain Chemlam® RL® RL1000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate

PSTGQZ215 / 68729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.