MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Haynes 263® alloy, cold rolled sheet, solution treated and aged
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excellent forming and welding characteristics. Applications include aircraft and land-based turbine engine applications, low-temperature combustors, transition liners, and some ring components.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS N06231, AMS 5872, AMS 5886
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.36 g/cc0.302 lb/in³a RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1050 MPa152000 psi
 88.0 MPa
@Temperature 1095 °C
12800 psi
@Temperature 2003 °F
 170 MPa
@Temperature 980 °C
24700 psi
@Temperature 1800 °F
 350 MPa
@Temperature 870 °C
50800 psi
@Temperature 1600 °F
 725 MPa
@Temperature 760 °C
105000 psi
@Temperature 1400 °F
 835 MPa
@Temperature 650 °C
121000 psi
@Temperature 1200 °F
 855 MPa
@Temperature 540 °C
124000 psi
@Temperature 1000 °F
Tensile Strength, Yield 635 MPa
@Strain 0.2 %
92100 psi
@Strain 0.2 %
 37.0 MPa
@Strain 0.2 %,
Temperature 1095 °C
5370 psi
@Strain 0.2 %,
Temperature 2003 °F
 87.0 MPa
@Strain 0.2 %,
Temperature 980 °C
12600 psi
@Strain 0.2 %,
Temperature 1800 °F
 220 MPa
@Strain 0.2 %,
Temperature 870 °C
31900 psi
@Strain 0.2 %,
Temperature 1600 °F
 515 MPa
@Strain 0.2 %,
Temperature 760 °C
74700 psi
@Strain 0.2 %,
Temperature 1400 °F
 525 MPa
@Strain 0.2 %,
Temperature 650 °C
76100 psi
@Strain 0.2 %,
Temperature 1200 °F
 540 MPa
@Strain 0.2 %,
Temperature 540 °C
78300 psi
@Strain 0.2 %,
Temperature 1000 °F
Elongation at Break 35.7 %35.7 %in 51 mm
 33.1 %
@Temperature 760 °C
33.1 %
@Temperature 1400 °F
in 51 mm
 35.6 %
@Temperature 650 °C
35.6 %
@Temperature 1200 °F
in 51 mm
 38.6 %
@Temperature 540 °C
38.6 %
@Temperature 1000 °F
in 51 mm
 54.7 %
@Temperature 870 °C
54.7 %
@Temperature 1600 °F
in 51 mm
 58.7 %
@Temperature 1095 °C
58.7 %
@Temperature 2003 °F
in 51 mm
 71.8 %
@Temperature 980 °C
71.8 %
@Temperature 1800 °F
in 51 mm
Modulus of Elasticity 221 GPa32100 ksiRT
 143 GPa
@Temperature 1000 °C
20700 ksi
@Temperature 1830 °F
 154 GPa
@Temperature 900 °C
22300 ksi
@Temperature 1650 °F
 166 GPa
@Temperature 800 °C
24100 ksi
@Temperature 1470 °F
 176 GPa
@Temperature 700 °C
25500 ksi
@Temperature 1290 °F
 185 GPa
@Temperature 600 °C
26800 ksi
@Temperature 1110 °F
 192 GPa
@Temperature 500 °C
27800 ksi
@Temperature 932 °F
 198 GPa
@Temperature 400 °C
28700 ksi
@Temperature 752 °F
 205 GPa
@Temperature 300 °C
29700 ksi
@Temperature 572 °F
 212 GPa
@Temperature 200 °C
30700 ksi
@Temperature 392 °F
 219 GPa
@Temperature 100 °C
31800 ksi
@Temperature 212 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000115 ohm-cm0.000115 ohm-cmRT
 0.000116 ohm-cm
@Temperature 100 °C
0.000116 ohm-cm
@Temperature 212 °F
 0.000118 ohm-cm
@Temperature 200 °C
0.000118 ohm-cm
@Temperature 392 °F
 0.000120 ohm-cm
@Temperature 300 °C
0.000120 ohm-cm
@Temperature 572 °F
 0.000122 ohm-cm
@Temperature 400 °C
0.000122 ohm-cm
@Temperature 752 °F
 0.000124 ohm-cm
@Temperature 500 °C
0.000124 ohm-cm
@Temperature 932 °F
 0.000124 ohm-cm
@Temperature 900 °C
0.000124 ohm-cm
@Temperature 1650 °F
 0.000124 ohm-cm
@Temperature 1000 °C
0.000124 ohm-cm
@Temperature 1830 °F
 0.000125 ohm-cm
@Temperature 800 °C
0.000125 ohm-cm
@Temperature 1470 °F
 0.000126 ohm-cm
@Temperature 600 °C
0.000126 ohm-cm
@Temperature 1110 °F
 0.000126 ohm-cm
@Temperature 700 °C
0.000126 ohm-cm
@Temperature 1290 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.1 µm/m-°C
@Temperature 25.0 - 100 °C
6.17 µin/in-°F
@Temperature 77.0 - 212 °F
 12.1 µm/m-°C
@Temperature 25.0 - 200 °C
6.72 µin/in-°F
@Temperature 77.0 - 392 °F
 12.7 µm/m-°C
@Temperature 25.0 - 300 °C
7.06 µin/in-°F
@Temperature 77.0 - 572 °F
 12.8 µm/m-°C
@Temperature 25.0 - 400 °C
7.11 µin/in-°F
@Temperature 77.0 - 752 °F
 13.6 µm/m-°C
@Temperature 25.0 - 500 °C
7.56 µin/in-°F
@Temperature 77.0 - 932 °F
 18.1 µm/m-°C
@Temperature 1000 °C
10.1 µin/in-°F
@Temperature 1830 °F
Thermal Conductivity 11.7 W/m-K81.2 BTU-in/hr-ft²-°FRT
 13.0 W/m-K
@Temperature 100 °C
90.2 BTU-in/hr-ft²-°F
@Temperature 212 °F
 14.7 W/m-K
@Temperature 200 °C
102 BTU-in/hr-ft²-°F
@Temperature 392 °F
 16.3 W/m-K
@Temperature 300 °C
113 BTU-in/hr-ft²-°F
@Temperature 572 °F
 18.0 W/m-K
@Temperature 400 °C
125 BTU-in/hr-ft²-°F
@Temperature 752 °F
 19.7 W/m-K
@Temperature 500 °C
137 BTU-in/hr-ft²-°F
@Temperature 932 °F
 21.4 W/m-K
@Temperature 600 °C
149 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 23.0 W/m-K
@Temperature 700 °C
160 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 24.7 W/m-K
@Temperature 800 °C
171 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 26.8 W/m-K
@Temperature 900 °C
186 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 28.5 W/m-K
@Temperature 1000 °C
198 BTU-in/hr-ft²-°F
@Temperature 1830 °F
Melting Point 1300 - 1355 °C2370 - 2471 °F
Solidus 1300 °C2370 °F
Liquidus 1355 °C2471 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.60 %<= 0.60 %
Carbon, C 0.060 %0.060 %
Chromium, Cr 20 %20 %
Cobalt, Co 20 %20 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe <= 0.70 %<= 0.70 %
Manganese, Mn <= 0.60 %<= 0.60 %
Molybdenum, Mo 6.0 %6.0 %
Nickel, Ni 52 %52 %As Remainder
Silicon, Si <= 0.40 %<= 0.40 %
Titanium, Ti <= 2.4 %<= 2.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® 80 A UNS N07080 Nickel Superalloy
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Special Metals NIMONIC® Alloy 263
Special Metals NIMONIC® Alloy 80A
ATI Allvac® 718Plus™ Nickel Superalloy

NH263A / 16630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.