MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI LATISTAT 87/28-09 G/20 Polycarbonate, 20% Glass Fiber Reinforced Conductive Plastic  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 20% Glass Filled

Material Notes: Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable mechanical properties. The LATISTAT compounds are used in all applications where product surface must be completely and permanently free of static charges. Addition of carbons supplying electric semi-conductivity will diminish the flowability and good surface finish of the materials, and limiting the prospects of obtaining colored products.

Applications: cabinets, containers, boxes for storage and handling of discharge-sensitive electronic components, casings and bodies for electrical and mechanical components to be used in areas where flammable and explosive materials are processed, parts for typewriters, printers, photocopiers, parts for textile machinery, racks and tracks for printed circuits; electro-medical equipment.

Specific Notes for this Material: polycarbonate base (PC); good antistatic properties; 20% glass fiber; high dimensional stability.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inLATI
Linear Mold Shrinkage, Transverse 0.0030 cm/cm0.0030 in/inLATI
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 100 MPa14500 psiISO 527
Flexural Modulus 7.30 GPa1060 ksiASTM D790
Izod Impact, Notched 0.450 J/cm
@Temperature 23.0 °C
0.843 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 93
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C270 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °FASTM D648
Vicat Softening Point 140 °C284 °F50°C/h 50N; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 100 - 120 °C212 - 248 °F
Drying Temperature 110 - 120 °C230 - 248 °FNecessary, temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourNecessary, drying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics TR-2000 Block Insulation
Sinotek Materials Graphite Sealing Strip Fireproofing Sealing Products
Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade
RTP Company RTP 399 X 132891 C Polycarbonate (PC); ESD Protection - Electrically Conductive
RTP Company EMI 2560.6 Polycarbonate/ABS Alloy (PC/ABS); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PLATI222 / 50220

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.