MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hogen HM1100 Tungsten-Based Metal
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Slightly Magnetic.

Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduces soldering or erosion problems. To increase the machinability of this brittle metal, alloying elements are added and practical use of tungsten is possible for die casting tools.

Used in resistance brazing and high temp applications. Used as counter weights and counter balances, radiation shielding components, tool shanks for boring bars and other tools for chatter-free machining.

Data provided by Hogen Industries.

Key Words: Hogen Industries Class 1 Tungsten Alloys; AMS 7725B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 17.0 g/cc0.614 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 3232
Tensile Strength, Ultimate 827 MPa120000 psi
Tensile Strength, Yield 610 MPa
@Strain 0.2 %
88500 psi
@Strain 0.2 %
Elongation at Break 10 %10 %in 50 mm
Modulus of Elasticity 310 GPa45000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.61 µm/m-°C
@Temperature 20.0 - 400 °C
2.56 µin/in-°F
@Temperature 68.0 - 752 °F
Thermal Conductivity 75.0 W/m-K521 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Iron, Fe 3.0 %3.0 %
Nickel, Ni 7.0 %7.0 %
Tungsten, W 90 %90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PSM Industries PolyAlloys WNF-2109 Tungsten Heavy Alloy
Astaras ANVILOY® 1150 Tungsten Based High Temp Alloy
Aremco Ceramacast™ 646 Castable Ceramic
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite
W2Mo Tungsten Alloy

NHOG25 / 17333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.