MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Buna CB 22 Rubber, Cabo
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Buna CB 22 is a solution high-cis polybutadiene polymer produced with neodymium catalyst

Production Plant: Cabo de Santo Agostinho-PE-Brazil

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Mooney Viscosity 6363[ME]; ASTM D1645
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month
@Temperature <=40.0 °C
18.0 Month
@Temperature <=104 °F
 
Descriptive Properties
Content>96%cis 1.4 content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Buna CB 22 Rubber, TX
Lanxess Buna CB 728 T Rubber, TX
Lanxess Buna CB 45 Rubber (Texas Plant)
Lanxess Buna CB 22 Rubber, Singapore
Lanxess Buna CB 22 Rubber, Port Jerome

PLANY8485 / 208878

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.