MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description

POLYBATCH® 8153/UV2 is a white/UV masterbatch based in polyethylene. This product has been specifically engineered to provide dispersion and opacity at a competitive cost with good distributive letdown mixing. POLYBATCH® 8153/UV2 is recommended for use in outdoor film, sheet, and molding applications.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.57 g/cc1.57 g/ccASTM D792
Moisture Absorption <= 0.100 %<= 0.100 %ASTM D789
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 58 %58 %
 
Descriptive Properties
Pellet Count 40pellets/gram

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell WL-38 40% Glass and Mineral Reinforced PET
A. Schulman POLYBATCH™ White LL8000 AP Concentrate Based In LLDPE
A. Schulman POLYBATCH™ White 8350 EC1 Concentrate Based In LDPE
A. Schulman POLYBATCH™ White 8000 AP Concentrate Based In LDPE
A. Schulman POLYBATCH™ Bright White LL80250 Concentrate Based In LLDPE

PASHU492 / 25456

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.