MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schott LG-750 Phosphate Laser Glass
Categories: Ceramic; Glass; Optical

Material Notes: LG-750 is the potassium-barium-aluminum-phosphate based glass with a high cross section for stimulated emission, low nonlinear refractive index, and good thermal characteristics. This glass was initially developed for the US DOE NOVA Laser Facility. The glass property space of this glass is extensively discussed in “Effect of composition on the thermal, mechanical, and optical properties of phosphate laser glasses” Proc SPIE, Vol 1277, 121-139 (1990).

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 3.03.0pH = 0.3 at 25 °C
Alkali Class, AR 3.03.0pH = 12 at 50 °C
Stain Resistance Class, FR 1.01.0pH = 4.6 100 h at 25 °C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 2902900.1/20
Modulus of Elasticity 50.1 GPa7270 ksi
Poissons Ratio 0.2560.256
Fracture Toughness 0.480 MPa-m½0.437 ksi-in½KIC
Shear Modulus 19.9 GPa2890 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  114 µm/m-°C
@Temperature 20.0 - 40.0 °C
63.3 µin/in-°F
@Temperature 68.0 - 104 °F
 130.1 µm/m-°C
@Temperature 20.0 - 300 °C
72.28 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.720 J/g-°C0.172 BTU/lb-°F
Thermal Conductivity  0.490 W/m-K
@Temperature 25.0 °C
3.40 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
 0.520 W/m-K
@Temperature 90.0 °C
3.61 BTU-in/hr-ft²-°F
@Temperature 194 °F
Transformation Temperature, Tg 450 °C842 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5261.526
 1.516
@Wavelength 1054 nm
1.516
@Wavelength 1054 nm
 1.524
@Wavelength 633 nm
1.524
@Wavelength 633 nm
Transmission, Visible 68.2 %68.2 %
 
Descriptive Properties
Climatic resistance2Water Vapor at 40 – 50 °C for 30 h
Thermal Diffusivity2.43 [10-7 m2/sec]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Schott IRG 22 Infrared Chalcogenide Glass
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Hot-Rolled - Transverse Properties
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Hot-Rolled - Longitudinal Properties
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Hot-Rolled
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Cold-Rolled - Transverse Properties

CSGT9938 / 183191

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.