MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Ti-8V-5Fe-1Al, STA
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Characteristics: Metastable beta alloy, very high tensile and shear strengths.

Applications: Aerospace fasteners.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.65 g/cc0.168 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 1448 MPa>= 210000 psi
Tensile Strength, Yield >= 1380 MPa>= 200000 psi
Elongation at Break >= 6.0 %>= 6.0 %
Reduction of Area >= 12 %>= 12 %
Tensile Modulus 114 GPa16500 ksi
 100 GPa
@Temperature 315 °C
14500 ksi
@Temperature 599 °F
Shear Strength 793 MPa115000 psi
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.80 - 1.5 %0.80 - 1.5 %
Carbon, C <= 0.050 %<= 0.050 %
Iron, Fe 4.0 - 6.0 %4.0 - 6.0 %
Nitrogen, N <= 0.070 %<= 0.070 %
Oxygen, O 0.25 - 0.50 %0.25 - 0.50 %
Titanium, Ti 86 %86 %
Vanadium, V 7.5 - 8.5 %7.5 - 8.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-15Mo-5Zr-3Al Duplex Aged
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Solution Treated
Titanium Beta-CEZ ST 830°C (1525°F), Aged 550°C
Titanium Ti-15Mo-5Zr ST 730°C, Aged 400°C
Titanium Ti-6Al-2Sn-4Zr-6Mo (Ti-6-2-4-6) STA-2

MTB851a / 142965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.