MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem PB681/59 Blown Film Extrusion Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Description: PB681/59 is a grade produced under high pressure in a tubular reactor. This resin is used for laminating films mainly on paper substrate. It is also used in the extrusion coating process. Films obtained with this product show excellent optical properties and high draw down ability

Automatic packaging for several products; Lamination.

Additives: Antiblock, D and Slip High

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.922 g/cc0.922 g/ccASTM D1505/D792
Thickness 38.0 microns1.50 mil
Melt Flow 3.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 340 %340 %ASTM D882
Film Elongation at Break, TD 1050 %1050 %ASTM D882
Elmendorf Tear Strength TD 100 g100 ggF; ASTM D1922
Dart Drop Test 60.0 g0.132 lbgF/50%f; ASTM D1709
Film Tensile Strength at Break, MD 30.0 MPa4350 psiASTM D882
Film Tensile Strength at Break, TD 20.0 MPa2900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %
@Thickness 0.0380 mm
5.0 %
@Thickness 0.00150 in
ASTM D1003
Gloss 112 %
@Thickness 0.0380 mm
112 %
@Thickness 0.00150 in
60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Zone 1 110 °C230 °F
Die Temperature 150 °C302 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
Braskem PB681/59 LDPE Blown Film Extrusion Polyethylene
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Braskem EB853 Cast Film Extrusion Low Density Polyethylene

PBRAS730 / 109532

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.