MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Albis Plastics Polyethylene PE 11A3 GF33C , 33% Glass Fiber Chemically Coupled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Semi-crystalline Polyethylene (PE)

Characteristics: High Stiffness, Strength and Chemical Resistance

Applications: Appliances, Industrial Fittings, and Housings

Processing: Injection Molding (Melt Temperature: 410-575°F, Mold Temperature: 40-160°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.7 MPa8800 psiASTM D638
Elongation at Yield 2.5 %2.5 %ASTM D638
Flexural Yield Strength 89.6 MPa13000 psiASTM D790
Flexural Modulus 4.14 GPa600 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 302 °C410 - 576 °FInjection
Mold Temperature 4.00 - 71.0 °C39.2 - 160 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® HDPE E GF40 40% Glass Filled
Omni Plastics OmniTech™ HDPE GRC30 Glass Reinforced
Techmer ES HiFill® HDPE GF30 30% Glass Filled
Omni Plastics OmniTech™ HDPE GRC30 High Density Polyethylene, 30% Glass Reinforced
Omni Plastics OmniTech™ HDPE GRC40 Glass Reinforced

PZA1B65 / 21752

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.