MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sandvik H15F Extra-fine Grain Cemented Carbide for Rotary Tools  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: SANDVIK extra-fine grain cemented carbide grades have been developed to meet the exacting demands placed on solid carbide tooling by modern technology.

SANDVIK extra-fine grain cemented carbide grades are true submicron grain size tungsten carbide alloys. The tungsten carbide grain size is 0,8 µm, which is precisely controlled. These grade offer an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of toughness.

SANDVIK grade H15F incorporates 15% cobalt (Co) and 85% tungsten carbide (WC). H15F is recommended for solid carbide rotary tool applications in the ISO K30/K40 (USA C1-2) range.

It has special advantages where high toughness and sharp edge profiles are needed.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 13.95 g/cc0.5040 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 90.490.4
Hardness, Vickers 1400140030
Flexural Strength 4000 MPa580000 psiTransverse Rupture; ISO 3327
Compressive Strength 5350 MPa776000 psi
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 15 %15 %
WC 85 %85 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum - SiC Metal Matrix Composite
China Tungsten YG6A Tungsten Carbide for Cutting Tools
Sandvik C15C Cemented Carbide for hot rolling applications
Sandvik H11N 11% Cobalt Binder Cemented Carbide, Seal Grade
Sandvik H15F Cemented Carbide for Can Tooling

NSANDV034 / 18928

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.