MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

414 Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 400 Series Stainless Steel

Material Notes: 16 mm diameter bar, heated to 980°C for 30 minutes, oil quenched, tempered at 49°C.

Key Words: UNS S41400, AMS 5615, ASTM A276, ASTM A314, ASTM A473, ASTM A511, ASTM A580, FED QQ-S-763, SAE J405 (51414), martensitic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 459459Converted from Rockwell C Hardness
Hardness, Knoop 506506Converted from Rockwell C Hardness
Hardness, Rockwell C 4848before testing
Hardness, Vickers 487487Converted from Rockwell C hardness.
Tensile Strength, Ultimate 1795 MPa260300 psi
Tensile Strength, Yield 1013 MPa
@Strain 0.2 %
146900 psi
@Strain 0.2 %
Elongation at Break 15 %15 %in 50 mm
Tensile Modulus 200 GPa29000 ksi
Izod Impact 30.0 - 80.0 J22.1 - 59.0 ft-lbhardened and tempered
 70.0 - 110 J51.6 - 81.1 ft-lbannealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000700 ohm-cm
@Temperature 20.0 °C
0.0000700 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 0.000 - 100 °C
5.78 µin/in-°F
@Temperature 32.0 - 212 °F
 11.0 µm/m-°C
@Temperature 0.000 - 315 °C
6.11 µin/in-°F
@Temperature 32.0 - 599 °F
 12.1 µm/m-°C
@Temperature 0.000 - 540 °C
6.72 µin/in-°F
@Temperature 32.0 - 1000 °F
 12.4 µm/m-°C
@Temperature 0.000 - 650 °C
6.89 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  24.9 W/m-K
@Temperature 100 °C
173 BTU-in/hr-ft²-°F
@Temperature 212 °F
 28.7 W/m-K
@Temperature 500 °C
199 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1425 - 1480 °C2597 - 2700 °F
Solidus 1425 °C2597 °F
Liquidus 1480 °C2700 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 12.5 %12.5 %
Iron, Fe 83 %83 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 1.88 %1.88 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
410 Stainless Steel
420 Stainless Steel
416 Stainless Steel
304 Stainless Steel
405 Stainless Steel

MQ414A / 13013

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.