MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) HB5020 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: HB-5020 is a high molecular weight high density polyethylene.

Applications: extrusion blow molding

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow  0.22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.22 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 1.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
1.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
20 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.0 MPa3630 psiISO 527-1
Elongation at Yield 9.0 %9.0 %ISO 527-1
Tensile Modulus 1.00 GPa145 ksiISO 527-1
Tensile Impact Strength 100 kJ/m²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
ISO 8256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 78.0 °C172 °FISO 306
Heat Distortion Temperature  43.0 °C
@Pressure 1.80 MPa
109 °F
@Pressure 261 psi
ISO 57B-1
 75.0 °C
@Pressure 0.450 MPa
167 °F
@Pressure 65.3 psi
ISO 75A-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 131 °C268 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene
Iran Petrochemical (PCC) HB4265 High Density Polyethylene
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene
Iran Petrochemical (PCC) LF0250/KJ Low Density Polyethylene

PIPC239 / 149701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.