MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Moplen HP548S Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: LyondellBasell Australias polypropylene grade HP548S is a high flow homopolymer with a modified molecular weight distribution. It is formulated with a general-purpose additive package and nucleant. HP548S has been formulated for use in thin walled packaging containers, caps and closures where rapid cycle times and enhanced rigidity are required. Applications: Caps & Closures, Containers, TWIM Food Containers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³Method D; ISO 1183-1
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ISO 868
Tensile Strength, Yield 33.0 MPa4790 psiISO 527-1,-2
Flexural Modulus 1.45 GPa210 ksiISO 178
Izod Impact, Notched (ISO) 2.30 kJ/m²
@Temperature 23.0 °C
1.09 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 150 °C302 °FISO 306
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NIZHNEKAMSKNEFTEKHIM PP 1548S (H32GA) Propylene Homopolymer
LyondellBasell Moplen HP548R Polypropylene
LyondellBasell Moplen HP548N Polypropylene
LyondellBasell Moplen HP548L Polypropylene
LyondellBasell Moplen EP548V Polypropylene, Impact Modified; Molded/Extruded

PEQT9041 / 220672

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.