MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

Multibase C6-530 Dow-Corning Class VI Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Multibase

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³Relative, no post cure; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030no post cure; ASTM D2240
 3131post cured-2 hours at 177°C; ASTM D2240
 3232post cured-4 hours at 177°C; ASTM D2240
 3333post cured- 8 hours at 177°C; ASTM D2240
Tensile Strength, Ultimate 8.20 MPa1190 psino post cure; ASTM D412
 8.301 MPa1204 psipost cured- 8 hours at 177°C; ASTM D412
 8.515 MPa1235 psipost cured- 4 hours at 177°C; ASTM D412
 9.087 MPa1318 psipost cured- 2 hours at 177°C; ASTM D412
Tensile Strength, Yield 0.889 MPa129 psiat 200%, no post cure- press cured for 5 minutes; ASTM D412
 1.05 MPa152 psi200%, post cured- 4 hours at 177°C; ASTM D412
 1.10 MPa160 psi200%, post cured- 8 hours at 177°C; ASTM D412
 1.15 MPa167 psiat 200%, post cured- 2 hours at 177°C; ASTM D412
Elongation at Break 793 %793 %post cured- 4 hours at 177°C; ASTM D412
 796 %796 %post cured- 8 hours at 177°C; ASTM D412
 831 %831 %no post cure; ASTM D412
 833 %833 %post cured- 2 hours at 177°C; ASTM D412
Tear Strength 26.3 kN/m150 pliDie B, post cured- 4 hours at 177°C; ASTM D624
 27.0 kN/m154 pliDie B, post cured- 8 hours at 177°C; ASTM D624
 27.5 kN/m157 pliDie B, no post cure; ASTM D624
 28.2 kN/m161 pliDie B, post cured- 2 hours at 177°C; ASTM D624
Compression Set 46 %46 %no post cure; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.0 %2.0 %no post cure
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase C6-515 Dow-Corning Class VI Elastomer
Dow 25150-G SILICONE RUBBER
Dow HV 1650/50 SILICONE RUBBER
Dow Silastic® 1604-T SILICONE RUBBER
Dow HV 1520/50 KIT PARTS A&B

PMULTI177 / 54081

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.