MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Sumitomo Bakelite NEONIT® SK60 L8F Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: NEONIT® SK60 L8F is a medium flow long glass fiber reinforced epoxy molding compound with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over molding.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.86 g/cc0.0672 lb/in³ISO 1183
Apparent Bulk Density 0.500 g/cc0.0181 lb/in³ISO 60
Water Absorption 0.050 %0.050 %ISO 62
Linear Mold Shrinkage 0.00090 cm/cm0.00090 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 119 MPa17300 psiISO 527-1
Elongation at Break 0.80 %0.80 %ISO 527-1
Tensile Modulus 21.0 GPa3050 ksiISO 527-1
Flexural Strength 223 MPa32300 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Compressive Strength 227 MPa32900 psiISO 604
Charpy Impact, Notched 5.20 J/cm²24.7 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 38.0 kV/mm965 kV/inIEC 60112
Dissipation Factor 0.022
@Frequency 1e+6 Hz
0.022
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 8.00 µm/m-°C4.44 µin/in-°FTMA
CTE, linear, Transverse to Flow 59.0 µm/m-°C32.8 µin/in-°FTMA
Thermal Conductivity 0.560 W/m-K3.89 BTU-in/hr-ft²-°FASTM E1461
Glass Transition Temp, Tg 165 °C329 °FTMA
Shrinkage -0.0400 %-0.0400 %Post; ISO 2577
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound
Sumitomo Bakelite NEONIT® SK80 L8G Epoxy Molding Compound
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Epoxy Technology EPO-TEK® H70E-TI Thermally Conductive, Electrically Insulating Epoxy
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound

PSUMIT175 / 193980

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.