MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Applied Composites 8049 Polyester SMC
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: Industry Application: High Strength
Product Application: Military
Distinct Features: High Impact Low Profile; Paintable/In Mold Coatable; Low Shrink; Low Moisture Absorption; Bondable; Formulated for High Stress and Vibration

Information provided by Applied Composites Corporation.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %ASTM D570
Linear Mold Shrinkage 0.00 cm/cm0.00 in/inCold Part VS Cold Tool; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 4545ASTM D2583
Tensile Strength, Ultimate 103 MPa15000 psiASTM D638
Tensile Modulus 12.4 GPa1800 ksiASTM D638
Flexural Strength 200 MPa29000 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiTangent; ASTM D790
Izod Impact, Notched 8.01 J/cm15.0 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Composites 150 Polyester SMC
Applied Composites 120 Polyester SMC
Applied Composites 8033 Polyester SMC
Applied Composites 179 Polyester SMC
Applied Composites 8072 Polyester SMC

PAPPLI10x / 24136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.