MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celcon® TX90PLUS Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: An M90 based material modified to provide significant improvement in impact strength and flexibility.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
Moisture Absorption at Equilibrium 0.80 %0.80 %ASTM D570
Linear Mold Shrinkage 0.017 cm/cm0.017 in/in
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Yield 41.0 MPa5950 psiASTM D638
Elongation at Break >= 250 %>= 250 %ASTM D638
Flexural Strength 49.0 MPa7110 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiASTM D790
Compressive Strength 61.0 MPa8850 psi10% Deflection; ASTM D695
Shear Strength 40.0 MPa5800 psiASTM D732
Izod Impact, Notched 1.30 J/cm2.44 ft-lb/inASTM D256
 1.00 J/cm
@Temperature -29.0 °C
1.87 ft-lb/in
@Temperature -20.2 °F
ASTM D256
Tensile Impact Strength 280 kJ/m²133 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® TX90 Acetal Copolymer
Avient Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Celanese 1000 Nylon 6/6, at 50% RH
Celanese 1503 Nylon 6/6, 33% Glass-Fiber Reinforced, at 50% RH
Kolon KOCETAL® K200 Standard Grade Acetal Resin

PHCU57 / 45797

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.