Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer
Categories:
Polymer
;
Thermoplastic
;
TPO
Material Notes:
Uses:
Flexible Grips; Footwear; General Purpose; Grommets; Handles; Industrial Applications; Soft Touch Applications; Toys
Injection Notes:
Injection Rate: Moderate-Fast
Extrusion Notes:
Screw Speed: 30 to 100 rpm
Information Provided by Teknor Apex
Key Words:
TPO
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.24
g/cc
1.24
g/cc
ASTM D792
Melt Flow
50
g/10 min
@Load 2.16 kg,
Temperature 190 °C
50
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
55
55
1 second; ASTM D2240
Tensile Strength at Break
5.17
MPa
750
psi
ASTM D412
Elongation at Break
650 %
650 %
ASTM D412
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
171
-
193
°C
340
-
380
°F
Middle Barrel Temperature
177
-
199
°C
350
-
390
°F
Front Barrel Temperature
182
-
204
°C
360
-
400
°F
Nozzle Temperature
188
-
210
°C
370
-
410
°F
Zone 1
166
-
188
°C
330
-
370
°F
Zone 2
171
-
193
°C
340
-
380
°F
Zone 3
177
-
199
°C
350
-
390
°F
Zone 5
182
-
204
°C
360
-
400
°F
Die Temperature
190
-
210
°C
374
-
410
°F
Melt Temperature
188
-
210
°C
370
-
410
°F
Processing Temperature
Mold Temperature
25.0
-
65.6
°C
77.0
-
150
°F
Injection Pressure
1.38
-
6.89
MPa
200
-
1000
psi
Back Pressure
0.172
-
0.345
MPa
25.0
-
50.0
psi
Cushion
0.381
-
2.54
cm
0.150
-
1.00
in
Screw Speed
50
-
100
rpm
50
-
100
rpm
Descriptive Properties
Appearance
Opaque
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aclo Accutech TPO TPO030T9V Paintable Grade
Noble Polymers Ecobarrier™ 0414 Thermoplastic Olefin (TPO)
Global TPE-LS64A Elastomer Grade
Teknor Apex Telcar® TL-2365A Thermoplastic Polyolefin Elastomer
Formosa Plastics Formolene® 2710A Injection Molding RTPO Polypropylene
PTEKNP487 / 129568
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.