MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: AboCoat 8401-1 A/B is a conventional highly-filled coating to produce conductive paths with the highest silver content possible. It requires strict controls. Resistivity may rise to 0.1 ohm/sq under unfavorable mixing, application, and atmospheric conditions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 81.5 %81.5 %
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.010 ohm<= 0.010 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 180 min
@Temperature 50.0 - 100 °C
0.500 - 3.00 hour
@Temperature 122 - 212 °F
Optional
 >= 1440 min
@Temperature 22.0 - 30.0 °C
>= 24.0 hour
@Temperature 71.6 - 86.0 °F
Pot Life 3000 min3000 min
 
Descriptive Properties
ColorGray
Metal (%)95.7of vehicle
Parts by Weight (pbw)100Part A Resin
 5Part B Hardener
ViscosityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboWeld 8505-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
Aremco Aremco-Bond™ 616 Electrically & Thermally Conductive Adhesive, Silver-Filled
GEHR Plastics Noryl PPO
Abatron AboCoat 8709-12/AboCure 50-12 Silver-Filled Electrically Conductive Epoxy Compound
Aremco Aremco-Bond™ 525 Electrically & Thermally Conductive Material, Silver Filled

PABC845 / 107829

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.