MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPV 4785B40 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4700 Series are very high flow injection molding engineering grades with excellent UV resistance, elasticity, and surface aesthetics designed for demanding automotive applications including window encapsulation and exterior parts. This product is a black, medium hardness, low density thermoplastic vulcanizate suited for injection molding applications that require superior flow properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Good Flexibility; Good Processability; High Flow; High Heat Resistance; Low Density; Low Specific Gravity; High Hardness; Low Compression Set

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: GM GMW15812P-TPV(EPMD+PP) Type 8M Color: Black; VAG VW501 23 Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Viscosity 190 cP
@Shear Rate 206 1/s,
Temperature 200 °C
190 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  84
@Time 5.00 sec
84
@Time 0.00139 hour
Extruded; ASTM D2240
 86
@Time 5.00 sec
86
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 8.89 MPa1290 psiFlow; ASTM D412
 9.51 MPa1380 psiAcross Flow; ASTM D412
 8.56 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
1240 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 9.13 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
1320 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  4.80 MPa
@Strain 100 %
696 psi
@Strain 100 %
Across Flow; ISO 37
 5.50 MPa
@Strain 100 %
798 psi
@Strain 100 %
Flow; ISO 37
 5.13 MPa
@Strain 100 %,
Treatment Temp. 150 °C
745 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 5.23 MPa
@Strain 100 %,
Treatment Temp. 135 °C
759 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 450 %450 %Flow; ASTM D412
 540 %540 %Across Flow; ASTM D412
 443 %
@Treatment Temp. 150 °C,
Time 605000 sec
443 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 464 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
464 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 40.3 kN/m230 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  32 %
@Temperature 22.8 °C,
Time 79200 sec
32 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 44 %
@Temperature 70.0 °C,
Time 79200 sec
44 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 72 %
@Temperature 125 °C,
Time 252000 sec
72 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 232 °C360 - 450 °FInjection
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® TPV 5790B Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X5750DB Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X5740DB Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X5735B Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X4750B42 Thermoplastic Vulcanizate

PTEKNQ1166 / 237657

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.