MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It features high temperature resistance and outstanding chemical resistance and is widely used in a variety of potting and encapsulation applications where thermal conductivity is needed. Aside from being a superior adhesive, sealant and coating, EP42HT-2AO-1 Black is castable to thicknesses exceeding 2-3 inches. EP42HT-2AO-1 Black cures readily at ambient temperatures or more quickly at elevated temperatures even in the presence of moisture. The cured epoxy compound is resistant to various types of chemicals such as inorganic and organic acids, alkalis, many organic solvents, aromatic hydrocarbons, etc. EP42HT-2AO-1 Black is an excellent electrical insulator. Especially noteworthy is its cryogenic serviceability from 4K up to +400°F combined with being relatively impervious to intermittent exposures to steam. Aside from its widespread use in the electronics industry, EP42HT-2AO-1 Black is also used in medical, fiber-optic, optical, as well as OEM type applications. While the mixed material is black in color, Part A is black and Part B is brown.

Product Advantages:

  • Non-critical 100:40 mix ratio by weight
  • Convenient cure schedules at both ambient and elevated temperatures
  • Excellent chemical resistance to acids, alkalis and many solvents
  • Castable to thicknesses exceeding 2-3 inches
  • Excellent flow properties
Key Features and Benefits:
  • Passes NASA low outgassing specifications
  • Outstanding thermal conductivity and electrical insulation properties
  • Superior thermal stability with serviceability up to +400°F
  • Suitable for cryogenic applications at temperatures down to 4KInformation provided by MasterBond®
Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 200 - 1000 cP200 - 1000 cPPart B
 50000 - 120000 cP50000 - 120000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength at Break >= 51.7 MPa>= 7500 psi
Elongation at Break >= 2.0 %>= 2.0 %
Tensile Modulus >= 3.45 GPa>= 500 ksi
Shear Strength >= 8.27 MPa>= 1200 psiTensile lap, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 - 30.0 µm/m-°C13.9 - 16.7 µin/in-°F
Thermal Conductivity 1.30 - 1.44 W/m-K9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -168 °C-270 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 93.3 °C
2.00 - 3.00 hour
@Temperature 200 °F
 1440 - 4320 min
@Temperature 23.9 °C
24.0 - 72.0 hour
@Temperature 75.0 °F
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
in unopened container
 
Descriptive Properties
Mixing Ratio (A to B)100:40by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Atom Adhesives AA-DUCT 905 Epoxy Adhesive
Master Bond EP42HT-2LTE Two Component Epoxy
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
DuPont Mobility and Materials Betamate™ XW 1185 Epoxy
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy

PMASTB399 / 149646

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.