MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the thermoplastic shell softens and the gas increases its pressure, resulting in an expansion of the spheres.

Applications: Anti-slip coatings; Printing ink; Car underbody coatings; Industrial non-woven textiles;

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 0.0120 g/cc<= 0.000434 lb/in³TMA
Particle Size 18 - 24 µm18 - 24 µmD(0.5)
 
Thermal PropertiesMetricEnglishComments
Transformation Temperature 138 - 148 °C280 - 298 °FExpansion Starting Temperature
 188 - 200 °C370 - 392 °FTemp at Max Expansion
 
Descriptive Properties
Solvent Resistance5Scale of 1 to 5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Amco PRIMATOP PP CO 100 NB High Impact Copolymer
Akzo Nobel Expancel® 930 MB 120 Masterbatch with unexpanded microspheres
Dow Surlyn® 7940 Ionomer Resin, Lithium
Akzo Nobel Expancel® 051 WU 40 Wet unexpanded microspheres
Akzo Nobel Expancel® 092 DU 40 Dry unexpanded microspheres

PEXPAN31 / 38088

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.