MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult injection molding applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

Key Features:

  • Used in glass encapsulation applications
  • Used in sealing applications.
  • Recommended for applications requiring superior part surface appearance.
  • Designed to be injected at lower molding temperatures or at lower injection pressures.
  • EU and China RoHS compliant.
Applications:
  • Automotive-Glass Encapsulation and Weather Seals
Uses:
  • Automotive Applications
  • Automotive Interior Trim
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 59592 mm, 15 sec; ISO 868
Tensile Strength at Break 4.83 MPa700 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 2.00 MPa290 psiAcross Flow; ASTM D412
Elongation at Break 480 %480 %Across Flow; ASTM D412
Compression Set  29 %
@Temperature 22.8 °C,
Time 252000 sec
29 %
@Temperature 73.0 °F,
Time 70.0 hour
ASTM D395
 56 %
@Temperature 125 °C,
Time 252000 sec
56 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -62.8 °C-81.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr79
ColorBlack
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
A. Schulman Alcryn® 1060 BK Melt Processable Rubber
ExxonMobil Santoprene® 101-45W255 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer

PADVA057 / 22747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.