Forms: Pellets
Filler/Reinforcement: Carbon Fiber, 30% Filler by Weight
Additive: PTFE Lubricant(15%)
Features: Lubricated, Good Wear Resistance and Low Friction
Appearance: Black
TPCI# 9441101