MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostalen ACP 9255 PLUS High Density Polyethylene (HDPE), Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Hostalen ACP 9255 Plus is a high density polyethylene resin which possesses an outstanding combination of stiffness and impact performance. Hostalen ACP 9255 Plus can be processed on blown film lines at high output rates with excellent bubble stability, very low gel levels and homogeneous appearance which converters and end-users require for high quality thin and thick film production. Hostalen ACP 9255 Plus can enable the production of films with a very broad conversion window, good lay flat properties and excellent roll configuration. Typical applications are lamination and release films, artificial paper, labels, bags and heavy duty packaging. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Food Packaging Film, Heavy Duty Packaging, Lamination Film, Products for Use in Property Modification

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ISO 1183-1
Melt Flow  0.40 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 400 %400 %ISO 527-1,-3
Film Elongation at Break, TD 470 %470 %ISO 527-1,-3
Tensile Modulus 1.35 GPa196 ksiISO 527-1,-2
Dart Drop Test >= 200 g>= 0.441 lb
Film Tensile Strength at Break, MD 75.0 MPa10900 psiISO 527-1,-3
Film Tensile Strength at Break, TD 65.0 MPa9430 psiISO 527-1,-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FISO 3146
Vicat Softening Point 76.0 °C169 °FISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 230 °C392 - 446 °F
 
Descriptive Properties
Processing MethodBlown Film
Test Specimenfilm properties tested using 20µm thickness at 220°C, long stalk process, blow up ratio 4:1.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostalen ACP 9254 Plus High Density Polyethylene (HDPE), Film Grade
LyondellBasell Hostalen ACP 9240 PLUS High Density Polyethylene (HDPE), Film Grade
LyondellBasell Luflexen hyPE 35P FA Polyethylene
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications
CPT C-Flex® R70-190 Opaque Biocompatible TPE

PEQT8459 / 220094

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.