MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF Capron® HPN 9233G HS BK-102 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Capron HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced nylon 6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times while maintaining excellent properties. It exhibits high strength, rigidity and heat resistance. Surface appearance has been improved, cycle times reduced and creep resistance retained. This heat stabilizer version extends the retention of mechanical properties at elevated temperatures while maintaining excellent chemical resistance to greases, oils and hydrocarbons.

Capron HPN 9233G HS BK-102 is generally recommended for applications such as window locks, valve bodies, chair shells, door and window hardware, connectors, switch components, relay parts, terminal blocks, power tool housings, gears, chainsaws, blowers, trimmer housings and ZZZ ASTM Callout PA220G 33A 43370.

Data provided by Allied Signal.

Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 270-295 degC (518-563 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO data
Water Absorption 1.1 %1.1 %24 hrs; ISO data
Moisture Absorption at Equilibrium 1.8 %1.8 %50% RH; 23°C; ISO data
Water Absorption at Saturation 6.4 %6.4 %in water; 23°C; ISO data
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM data MD
 0.013 cm/cm0.013 in/inISO data
Linear Mold Shrinkage, Transverse 0.017 cm/cm0.017 in/inISO Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 175 MPa25400 psiSame value from ASTM and ISO tests; 5 mm/min.
Elongation at Break 2.8 %2.8 %ISO, 5 mm/min
 3.0 %3.0 %ASTM, 5 mm/min
Flexural Yield Strength 265 MPa38400 psiASTM Data
Flexural Modulus 8.40 GPa1220 ksiISO Value
 9.38 GPa1360 ksiASTM Value
Poissons Ratio 0.350.35ISO data
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmISO data
Dielectric Strength 22.0 kV/mm559 kV/inISO data
 
Thermal PropertiesMetricEnglishComments
CTE, linear 38.0 µm/m-°C
@Temperature 20.0 °C
21.1 µin/in-°F
@Temperature 68.0 °F
ASTM data
Melting Point 220 °C428 °FASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 174 °C345 °FISO data
Deflection Temperature at 1.8 MPa (264 psi) 208 °C406 °FASTM Data
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FSee Materials Notes
Mold Temperature 80.0 °C176 °FSee Materials Notes
Drying Temperature 85.0 °C185 °FSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G2 10% Glass Filled PBT
Morgan Advanced Ceramics Bailey Bond Thermal Ceramic
BASF Ultradur® B 4300 G6 BK5110 30% Glass Filled PBT

PALD51 / 23945

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.