MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kraton® G1641 H (SEBS) Linear Triblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1641 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form identified:
Kraton G1641 HU - supplied as an undusted powder
Kraton G1641 HS - supplied as a dusted powder

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1641 H is used in compound formulations and as a modifier of thermoplastics. It may also find use in formulating adhesives, sealants, coatings and modified bitumens.

Applications: Compounding and Personal Hygiene; Adhesives, Sealant and Coatings; Impact Modification; Medical; Packaging and Polymod; and Personal Care

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.50 %<= 0.50 %KM 04
Viscosity 500 - 850 cP500 - 850 cP15% Toluene Solution at 25°C; BAM 922
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 52
@Time 10.0 sec
52
@Time 0.00278 hour
Measured on compression molded slabs; ASTM D2240
Tensile Strength >= 17.2 MPa>= 2490 psiMeasured on solution cast film from toluene; BAM 1245
Elongation at Break >= 800 %>= 800 %Measured on solution cast film from toluene; BAM 1245
300% Modulus 4.34 MPa
@Strain 300 %
629 psi
@Strain 300 %
Measured on solution cast film from toluene; BAM 1245
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.03-0.1%, KM 08
 Polystyrene32.3-33.7%, Measured on polymer before hydrogenation, KM 03
 Total Extractables<1.6%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G1654 H (SEBS) Linear Triblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer

PKRA9886 / 132785

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.